Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Izod Impact, Notched (ISO) = 28.1 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 59.0 kJ/m²
28.1 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics LNP LUBRILOY D2000 PC
LNP LUBRILOY* D2000 is a compound based on Polycarbonate resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant.
Izod Impact, Notched (ISO) 59.0 kJ/m²
28.1 ft-lb/in²
80*10*4; ISO 180/1A
SABIC Innovative Plastics Xenoy® 1731 PBT+PC
Impact/chemical resistant. UV-Stabilized. Excellent physical property retention in automotive exteriors and OVAD.
Izod Impact, Notched (ISO) 59.0 kJ/m²
28.1 ft-lb/in²
ISO 108/1A
Borealis Borcoat™ BB125E Polypropylene Adhesive for Steel Pipe Coating
Borcoat BB125E is a chemically modified polypropylene copolymer designed to be used as the tie layer between the epoxy corrosion protection layer and the top-coat polypropylene Borcoat BB108E-1199.B..
Izod Impact, Notched (ISO) 59.0 kJ/m²
28.1 ft-lb/in²
DAM; ISO 180/1A
DuPont Performance Polymers Zytel® ST7301 NC010 Nylon 6  (Unverified Data**)
Super Toughened Polyamide 6 Zytel ST7301 NC010 is a Super Tough heat stabilized lubricated polyamide 6 resin for injection molding and extrusion. It offers outstanding impact resistance over a wide ..
Copyright © lookpolymers.com All Rights Reserved