Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 27.9 kJ/m² @Thickness 4.00 mm, Temperature 23.0 °C |
13.3 ft-lb/in² @Thickness 0.157 in, Temperature 73.4 °F |
ISO 180 |
Azdel Plus C327-B01 31% Chopped Fiber Mat / PP Resin Matrix AZDEL® C327-B01 is a glass mat thermoplastic laminate based upon a random oriented chopped fiber mat contained within a polypropylene resin matrix. This composite material features high flow prope.. |