Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.70 - 4.70 kJ/m² @Temperature -40.0 - -40.0 °C |
1.76 - 2.24 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 4.03 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Glass/Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Glass/Mineral Reinforced". Each property range of values reported is minimum and maximum .. |