Polymer Property : Izod Impact, Notched (ISO) = 2.0543 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 4.3164 kJ/m²
2.0543 ft-lb/in²
ASTM D256
Daelim H&L Plavis G40 Aromatic Polyimide, 40% Graphite Filled, Machined Parts
Higher abrasion resistance than G15, high value stability and very low friction coefficient propertyInformation provided by Daelim H&L