Izod Impact, Notched (ISO) 14.2 kJ/m²
6.76 ft-lb/in²
GB/T 1843-2008
Sichuan Deyang Haton® hGR515 Polyphenylene Sulfide/PA Alloy
Injection molding, high strengthInformation provided by Sichuan Deyang Chemical Co., LTD