Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 120 kJ/m² | 57.1 ft-lb/in² | 80*10*4; ISO 180/1A |
SABIC Innovative Plastics LNP THERMOTUF R1000JX4 PA 66 (Asia Pacific) High Impact Nylon 66 compound containing Impact Modifier. |