Izod Impact, Notched (ISO) 12.6 kJ/m²

@Temperature -20.0 °C
6.00 ft-lb/in²

@Temperature -4.00 °F
ASTM D256
C.O.I.M. LARIPUR® LPR5850 Modified Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..
Izod Impact, Notched (ISO) 12.6 kJ/m²
6.00 ft-lb/in²
ISO 180-1A
Gromax CFG30-SN31N1 Nylon 6 30% Glass Filled (Dry)
Information provided by Gromax Enterprises Corp.