Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | >= 24.5 kJ/m² | >= 11.7 ft-lb/in² | |
Sibur ABS 2020 (30,31) Molding Grade ABS Plastic With high thermal and light resistance for automobile building, stable to atmospheric conditions in thermal and electric ageing, contacting with food products, as well as with compounding with PC. |
|||
Izod Impact, Notched (ISO) | 24.6 kJ/m² | 11.7 ft-lb/in² | ASTM D256 |
GEHR Plastics ECOGEHR® C-L Cellulose-Lignin Compound
(discontinued **) C-L is comprised of the wood components cellulose, natural fibers, lignin and fatty acids. It possesses many interesting properties that together are very similar to the natural wood. Consequently,.. |