Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 3.30 - 3.30 kJ/m² @Temperature -40.0 - -40.0 °C |
1.57 - 1.57 ft-lb/in² @Temperature -40.0 - -40.0 °F |
Average value: 3.30 kJ/m² Grade Count:1 |
Overview of materials for Polypropylene with 20% Calcium Carbonate (CaCO3) Filler This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene with 20% Calcium Carbonate (CaCO3) Filler". Each property range of values reported is mini.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Thickness >=5.00 mm |
1.57 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit II Phenolic, Paper Reinforcement, Dark Brown, Sheets Description: Mechanical and electrical applications used at normal air humidity. Very good electrical values.Information provided by Elektro-Isola |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Thickness >=5.00 mm |
1.57 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IIQ R Phenolic, Paper Reinforcement, Yellow, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Thickness >=5.00 mm |
1.57 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit IIQ R XX Phenolic, Paper Reinforcement, Yellow, Sheets Description: Mechanically a good Etronit type with electrical properties adequate for insulation in low-voltage applications. Applications: Used in electrical appliances, bus-bar carriers, partition.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Thickness >=5.00 mm |
1.57 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. The surfaces are grey as standard, but other colors can be selected from the color chart.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² @Thickness >=5.00 mm |
1.57 ft-lb/in² @Thickness >=0.197 in |
24hr/23°C/50% RH; ISO 180/2A; IEC/EN 60893-2 5.4.3 |
Elektro-Isola Etronit 201 MBM Phenolic/melamine, Paper Reinforcement, Grey/also other Colors, Sheets Description: This material is not standardized, but the base material is the same as Etronit 201 M. The surfaces consist of melamine, which ensures a scratch-resistant, tracking-resistant surface. T.. |
|||
Izod Impact, Notched (ISO) | 3.30 kJ/m² | 1.57 ft-lb/in² | ISO 180/1A |
Lucite International Elvakon® 4451 Super Low Gloss Acrylic Capstock Coextrusion grade developed to provide high aesthetic control, outstanding weatherability and impact and scratch resistance, the Elvakon® series enables protection of substrates with a durable prot.. |