Polymer Property : Izod Impact, Notched (ISO) = 1.20 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.52 kJ/m²
1.20 ft-lb/in²
ISO 180/1A
ExxonMobil PP1063L1 Polypropylene Homopolymer
Product Description: A homopolymer resin designed for general use. It is suitable for masterbatch carrier and other compounding applications and for the molding of caps, cups, containers and other ..