Polymer Property : Izod Impact, Notched (ISO) = 0.952 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 2.00 - 2.00 kJ/m²

@Temperature -30.0 - -30.0 °C
0.952 - 0.952 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 2.58 kJ/m² Grade Count:1
Overview of materials for Polystyrene, Molded, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene". Each property range of values reported is minimum and maximum values of appropriate MatWeb..