Mechanical Properties Metric English Comments
Izod Impact, Notched (ISO) 1.40 kJ/m²
0.666 ft-lb/in²
ISO 180/1A
Lucite International Diakon® Frost 902 70 Acrylic Polymer
Information provided by Lucite International
Izod Impact, Notched (ISO) 1.40 kJ/m²
0.666 ft-lb/in²
ISO 180/1A
Lucite International Diakon® Frost 902 80 Acrylic Polymer
Information provided by Lucite International