Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.550 kJ/m² @Temperature 23.0 °C |
0.262 ft-lb/in² @Temperature 73.4 °F |
ISO 180/A |
Victrex® PEEK 380P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli.. |