Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched (ISO) | 0.200 kJ/m² | 0.0952 ft-lb/in² | |
Lushan 2% WR-2 Wood Plastic Composites Compatibilizer Compatibilizer/coupling agent Lushan series for wood plastic composites is a maleic anhydride grafted polyolefins, applied in PE, PVC, wood powder, and bamboo powder and wood fiber composite materia.. |