Mechanical Properties Metric English Comments
Multi-axial Impact @ -30°C Total Energy 23.0 J
17.0 ft-lb
Energy to Peak Force (-22°F, Ductile Failure); ISO 6603-2
LyondellBasell Hifaxâ„¢ CA1110/2AC Thermoplastic Polyolefin Elastomer
Description: Hifaxâ„¢ CA1110/2AC Black medium high melt flow, 1,200 MPa flexural modulus, paintable thermoplastic elastomeric olefin (TEO) resin has a very good balance of processability, impact..