Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 21.0 - 200 kJ/m² @Temperature -20.0 - -20.0 °C |
9.99 - 95.2 ft-lb/in² @Temperature -4.00 - -4.00 °F |
Average value: 72.5 kJ/m² Grade Count:4 |
Overview of materials for Polypropylene, Mineral Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Mineral Reinforced". Each property range of values reported is minimum and maximum values.. |