Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 25.0 - 190 kJ/m²

@Temperature -30.0 - -30.0 °C
11.9 - 90.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 69.8 kJ/m² Grade Count:4
Overview of materials for Polybutylene Terephthalate (PBT), Glass Bead Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Glass Bead Filled". Each property range of values reported is minimum ..