Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 158 kJ/m²
75.2 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP LUBRICOMP LL002 PEEK