Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 71.0 kJ/m² | 33.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP QF006 PA 6/10 LNP THERMOCOMP* QF006 is a compound based on Nylon 6/10 resin containing 30% Glass Fiber. |
|||
Izod Impact, Unnotched (ISO) | 71.0 kJ/m² | 33.8 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOCOMP RC008H PA 66 LNP THERMOCOMP* RC008H is a compound based on Nylon 66 resin containing 40% Carbon Fiber. Added features of this material include: Electrically Conductive, Healthcare. |