Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 145 kJ/m² | 69.0 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP THERMOTUF VX99809 Super Tough Nylon Super Tough Nylon, Proprietary Filler(s), |
|||
Izod Impact, Unnotched (ISO) | >= 145 kJ/m² | >= 69.0 ft-lb/in² | Parallel to laminations; IEC 1212-2 5.5.3 |
Hippe EP PC 301 Woven Polyester Cloth Reinforced Epoxy Resin - Sheet Used in electrical and mechanical applications. Good resistance to SF6.Information provided by Hippe. |