Izod Impact, Unnotched (ISO) >= 500 kJ/m²
>= 238 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics Lexan® NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Izod Impact, Unnotched (ISO) >= 500 kJ/m²
>= 238 ft-lb/in²
80*10*3; ISO 180/1U
SABIC Innovative Plastics LNP FARADEX NX07331 PC+ABS (Asia Pacific)
FARADEX NX07331 is a commercial grade EMI shielding material
Izod Impact, Unnotched (ISO) 500 kJ/m²
238 ft-lb/in²
ASTM D4812
DuPont Performance Polymers Rynite® RE5231 BK533 Polyethylene Terephthalate (PET)
35% Glass/Mineral Reinforced Polyethylene TerephthalateRynite RE5231 BK533 is a 35% glass fiber/mica reinforced product modified for improved electrical properties such as dielectric strength.Inform..