Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 9.10 kJ/m² | 4.33 ft-lb/in² | |
Shandong Rike Chemical RIKE™ RK-764 MBS Impact Modifier for PVC Transparent Product Outline of MBS Impact ModifierRIKE™ MBS impact modifier for PVC transparent product developed by our R&D Center is a ternary copolymerized by Methyl Methacrylate, Butadiene and Styrene. It is endo.. |