Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 4.30 kJ/m² | 2.05 ft-lb/in² | ASTM D256 |
Tipco Tipcolite® TMS 111 Phenolic Compound, Cellulose Pulp, in fluffy form, having Soft Flow & High Strength Soft Flow Phenolic Compound, Reinforced with Cellulose Pulp, in fluffy formApplications: Defence ApplicationsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industrie.. |