Polymer Property : Izod Impact, Unnotched (ISO) = 26.7 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 26.7 - 137 kJ/m²
12.7 - 65.2 ft-lb/in²
Average value: 87.1 kJ/m² Grade Count:5
Overview of materials for Polycarbonate, PTFE Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, PTFE Filled". Each property range of values reported is minimum and maximum values of app..