Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 26.3 kJ/m² | 12.5 ft-lb/in² | ISO 180 |
LNP Thermocomp® EC-1006 Polyetherimide, Carbon Fiber Reinforcement
(discontinued **) Features: Good MoldabilityForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are st.. |