Polymer Property : Izod Impact, Unnotched (ISO) = 2.20 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Tipco Tipcolite® THD 311 Phenolic Compound, Wood Flour, having Medium Flow & High Strength
Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Electrical & ElectronicsProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India...
Izod Impact, Unnotched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Tipco Tipcolite® THR 211 Phenolic Compound, Asbestos Wood Flour & Minerals, Soft Flow & High Electrical Properties
Soft Flow Phenolic Compound, Reinforced with Asbestos Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industrie..
Izod Impact, Unnotched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Tipco Tipcolite® TX 211 Phenolic Compound, Wood Flour, having Medium Flow & High Electrical Properties
Medium Flow Phenolic Compound, Reinforced with Wood FlourApplications: Switchgear, HRC FusesProcessing: Compression MoldingInformation provided by the Manufacturer, Tipco Industries Ltd., India.
Izod Impact, Unnotched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Tipco Tipcolite® TX 311 Phenolic Compound, Wood Flour & Minerals, having Soft Flow & High Strength
Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd., I..
Izod Impact, Unnotched (ISO) 2.20 kJ/m²
1.05 ft-lb/in²
ASTM D256
Tipco Tipcolite® TX 312 Phenolic Compound, Wood Flour & Minerals having Soft Flow & Lower Density
Soft Flow Phenolic Compound, Reinforced with Wood Flour & MineralsApplications: Switchgear, HRC FusesProcessing: Injection MouldingInformation provided by the Manufacturer, Tipco Industries Ltd., I..