Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 25.0 - 35.0 kJ/m² | 11.9 - 16.7 ft-lb/in² | Average value: 31.7 kJ/m² Grade Count:3 |
Overview of materials for High Density Polyethylene (HDPE), Glass fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Glass fiber Filled". Each property range of values reported is minimum.. |
|||
Izod Impact, Unnotched (ISO) | 35.0 - 35.0 kJ/m² @Temperature -30.0 - -30.0 °C |
16.7 - 16.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 35.0 kJ/m² Grade Count:1 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |
|||
Izod Impact, Unnotched (ISO) | 25.0 - 35.0 kJ/m² @Temperature -30.0 - -30.0 °C |
11.9 - 16.7 ft-lb/in² @Temperature -22.0 - -22.0 °F |
Average value: 30.0 kJ/m² Grade Count:2 |
Overview of materials for Polyethylene Terephthalate (PET), 20% Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyethylene Terephthalate (PET), 20% Glass Reinforced". Specific grades with glass content between 15% .. |