Polymer Property : Izod Impact, Unnotched (ISO) = 129 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 8.00 - 129 kJ/m²
3.81 - 61.4 ft-lb/in²
Average value: 43.0 kJ/m² Grade Count:7
Overview of materials for Polymethylpentene, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polymethylpentene, Molded". Each property range of values reported is minimum and maximum values of appr..