Polymer Property : Izod Impact, Unnotched (ISO) = 128 kJ/m² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Izod Impact, Unnotched (ISO) 128 kJ/m²

@Temperature 23.0 °C
60.9 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP Stat-kon TE002
LNP* Stat-kon* TE002 is a compound based on Polyurethane resin containing Carbon Fiber. Added features of this material include: Electrically Conductive.This data was supplied by SABIC-IP for the A..
Izod Impact, Unnotched (ISO) 128 kJ/m²
60.9 ft-lb/in²
80*10*4; ISO 180/1U
SABIC Innovative Plastics LNP STAT-KON TE002 PU
LNP* STAT-KON* TE002 is a compound based on Polyurethane resin containing 10% Carbon Fiber. Added feature of this material is: Electrically Conductive.