Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 80.0 - 103 kJ/m² | 38.1 - 49.0 ft-lb/in² | Average value: 90.6 kJ/m² Grade Count:5 |
Overview of materials for Nylon 66, 50% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 50% Glass Fiber Filled". Specific grades with glass content between 45% and 54% are included. .. |