Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Unnotched (ISO) | 214 kJ/m² | 102 ft-lb/in² | 80*10*4; ISO 180/1U |
SABIC Innovative Plastics LNP LUBRICOMP RI001 PA 66 LNP* LUBRICOMP* RI001 is a compound based on Nylon 66 resin containing 2% Silicone. Added feature of this grade is: Wear Resistant. |