Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 76.88 MPa @Thickness 0.508 mm |
11150 psi @Thickness 0.0200 in |
1018 steel; ASTM C633-01 |
The NanoSteel® Company SHS 7574 HVOF Steel Alloy, Atomized Powder Coating Description: SHS 7574 HVOF is an iron based steel alloy with a nanoscale microstructure that features extreme corrosion resistance in high chlorine, salt fog, concentrated salt and seawater .. |