Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.924 MPa @Temperature 1400 °C, Time 10800 sec |
569.1 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ASM_36 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1400 °C, Time 10800 sec |
569.1 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ASM-35 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1500 °C, Time 10800 sec |
569.1 psi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories ASM-38 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1500 °C, Time 10800 sec |
569.1 psi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories ASM-39 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1500 °C, Time 10800 sec |
569.1 psi @Temperature 2730 °F, Time 3.00 hour |
|
Chosun Refractories ASM-40 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1400 °C, Time 10800 sec |
569.1 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ZM-2 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1400 °C, Time 10800 sec |
569.1 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ASM-37 Air-Setting Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Adhesive Bond Strength | 3.924 MPa @Temperature 1400 °C, Time 10800 sec |
569.1 psi @Temperature 2550 °F, Time 3.00 hour |
|
Chosun Refractories ZM-1 Special Mortar Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |