Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 3.50 MPa @Temperature 93.0 °C |
508 psi @Temperature 199 °F |
Tensile Lap Shear |
Henkel Hysol EA 9313 Paste Adhesive System Very low viscosity adhesive yielding tough, flexible bonds. Injectable. |