Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 5.90 MPa @Temperature 23.9 °C |
856 psi @Temperature 75.0 °F |
on ABS; ASTM D1002-64 |
3M Pronto™ CA-50 Gel Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high-viscosity gel consistenc.. |
|||
Adhesive Bond Strength | 5.90 MPa @Temperature 121 °C |
856 psi @Temperature 250 °F |
tube shears |
Henkel Hysol MA 560 Core Splice Adhesive A modified epoxy, low density (24-25 psf) foaming film adhesive capable of expanding 2.5 times the original thickness. Cures at 250°F / 121°C or 350°F / 177°C and is designed for service at temp.. |