Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 5.80 MPa @Temperature 25.0 °C |
841 psi @Temperature 77.0 °F |
tube shears |
Henkel Hysol MA 562SFR Core Splice Adhesive Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Flame-retardant, nonmetallic, medium tack, excellent slump resistance. |