Mechanical Properties Metric English Comments
Adhesive Bond Strength 26.9 MPa

@Temperature 25.0 °C
3900 psi

@Temperature 77.0 °F
Lap Shear
Henkel Hysol PL 795 Film Adhesive
Epoxy film adhesive designed for composite bonding applications. May cure at 250°F / 121°C or 350°F / 177°C, with service temperatures up to 350°F / 177°C. Ideal for co-cure or secondary bondi..