Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 21.0 MPa @Temperature -55.0 °C |
3050 psi @Temperature -67.0 °F |
Lap Shear |
Henkel Hysol EA 9681 Film Adhesive Epoxy film adhesive for bonding applications. Hysol EA9681 is formulated to provide excellent performance properties for many bonding applications, and has excellent results on composite surfaces th.. |