Polymer Property : Adhesive Bond Strength = 23.5 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Adhesive Bond Strength 23.5 MPa

@Temperature -55.0 °C
3410 psi

@Temperature -67.0 °F
Tensile Lap Shear
Henkel Hysol EA 9320NA Paste Adhesive System
High shear and high peel adhesive system with room temperature cure.