Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 14.0 MPa @Temperature 121 °C |
2030 psi @Temperature 250 °F |
Lap Shear |
Henkel Hysol PL 696 Film Adhesive Epoxy-based structural film adhesive designed primarily for out-of-autoclave curing process applications requiring low cure temperatures as well as low curing pressures and is also available in ligh.. |