Mechanical Properties Metric English Comments
Adhesive Bond Strength 8.20 MPa

@Temperature 25.0 °C
1190 psi

@Temperature 77.0 °F
tube shears
Henkel Hysol MA 557 Core Splice Adhesive
Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Designed to seal, splice or reinforce honeycomb materials. Excellent slump resistance, medium tack, n..
Adhesive Bond Strength 8.20 MPa

@Temperature 25.0 °C
1190 psi

@Temperature 77.0 °F
tube shears
Henkel Hysol MA 560 Core Splice Adhesive
A modified epoxy, low density (24-25 psf) foaming film adhesive capable of expanding 2.5 times the original thickness. Cures at 250°F / 121°C or 350°F / 177°C and is designed for service at temp..