Adhesive Bond Strength 7.30 MPa

@Temperature 121 °C
1060 psi

@Temperature 250 °F
tube shears
Henkel Hysol MA 557 Core Splice Adhesive
Modified epoxy foaming adhesive that may be cured at 250°F / 121°C or 350°F / 177°C. Designed to seal, splice or reinforce honeycomb materials. Excellent slump resistance, medium tack, n..