Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Adhesive Bond Strength | 0.724 MPa @Temperature 23.9 °C |
105 psi @Temperature 75.0 °F |
on nitrile rubber; ASTM D1002-64 |
3M Pronto™ CA-50 Gel Instant Adhesive One-part, room-temperature curing adhesive that is ready-to-use without metering or mixing. Bonded parts reach handling strength in 5-10 seconds on many applications.A high-viscosity gel consistenc.. |