Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Notched Tensile Strength = 2083 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Notched Tensile Strength 2083 MPa
302100 psi
K<sub>t</sub>7; 282°C Temper Temperature
Latrobe Lescalloy® 4330+V VAC-ARC High Strength Alloy Steel
LESCALLOY 4330+V VAC-ARC steel is a modification of 4330 steel with hardenability and other properties improved by the addition of vanadium. It is a low alloy steel capable of being heat treated to ..
Copyright © lookpolymers.com All Rights Reserved