Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Notched Tensile Strength | 1986 MPa | 288000 psi | K<sub>t</sub> = 10 |
Carpenter Custom 450® Stainless Steel, Condition H950 (Age Hardened 510°C) Data provided by Carpenter Technology Corporation.Custom 450® stainless is a martensitic age-hardenable stainless steel which exhibits very good corrosion resistance (similar to that of Stainless T.. |