Polymer Property : Charpy Impact Unnotched = 88.0 ft-lb/in² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 18.5 J/cm²

@Temperature -30.0 °C
88.0 ft-lb/in²

@Temperature -22.0 °F
Conditioned; ISO 179/1eU
Lanxess Durethan® DP 2801 000000 Nylon 66
PA 66 injection molding grade, non-reinforced, UL 94V-2 off 0,75 mm (listed), GWFI: 960°C off 0.75 mm, GWIT: 775°C off 0,75 mm, halogen-free