Polymer Property : Charpy Impact Unnotched = 85.0 J/cm² Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Charpy Impact Unnotched 85.0 J/cm²

@Temperature 316 °C
405 ft-lb/in²

@Temperature 600 °F
International Mold Steel DH21 Die Cast & Forging Steel
DH21 is for aluminum die cast dies.Information provided by International Mold Steel