Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 17.5 J/cm² @Temperature 23.0 °C |
83.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 LI PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |
|||
Charpy Impact Unnotched | 17.5 J/cm² @Temperature 23.0 °C |
83.3 ft-lb/in² @Temperature 73.4 °F |
|
Plastcom SLOVAMID 66 LI TS PA66, improved strength FeaturesModified with thermoplastic reactive caoutchouc, determined for mouldings with high toughness also at minus temperatures. Eligible application for ski-shoes, helmets for sport and other safe.. |