Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 8.10 J/cm² @Temperature 23.0 °C |
38.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1010GH30 NAT PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact Unnotched | 8.10 J/cm² @Temperature 23.0 °C |
38.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1013G30 1 NA PA6-GF30 30% Glass Reinforced, Injection Molding |
|||
Charpy Impact Unnotched | 8.10 J/cm² @Temperature 23.0 °C |
38.5 ft-lb/in² @Temperature 73.4 °F |
dry; ISO 179/1eU |
DSM Novamid® 1013GH30 1 NA/BK701 PA6-GF30 30% Glass Reinforced, Heat Stabilized, Injection Molding |
|||
Charpy Impact Unnotched | 8.10 J/cm² @Temperature 23.0 °C |
38.5 ft-lb/in² @Temperature 73.4 °F |
50%RH; ISO 179/1eU |
DuPont Performance Polymers Zytel® 80G25HS BK117 Nylon 66
(Unverified Data**) Zytel® 80G25HS BK117 is a 25% glass fiber reinforced, toughened, heat stabilized, black polyamide 66 resin for injection molding.Information provided by DuPont Performance Polymers |