Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Charpy Impact Unnotched | 7.70 J/cm² @Temperature -20.0 °C |
36.6 ft-lb/in² @Temperature -4.00 °F |
ISO 179/1eU |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |